Describe ammonia production from natural gas.
Answer. Desulphurised natural gas is steam-reformed to syngas, air is added in a secondary reformer to supply nitrogen, CO is shifted to CO₂ and H₂, CO₂ is removed, traces of CO/CO₂ are methanated, and the 3:1 H₂/N₂ gas is compressed and converted over iron catalyst.
Why. Each step prepares a clean hydrogen–nitrogen mixture; oxygen compounds poison the ammonia catalyst.
How.
- Primary reformer: Ni catalyst in tubes ~800 °C, steam/carbon ratio ~3.
- Secondary reformer: air burns some H₂, raising temperature; adds N₂.
- HT shift (Fe–Cr ~350–400 °C), LT shift (Cu–Zn ~200 °C).
- CO₂ removal (Benfield, aMDEA) — CO₂ goes to urea.
- Synthesis loop 150–200 bar, refrigeration to condense NH₃.
How is urea made? What is biuret and why is it controlled?
Answer. NH₃ and CO₂ react at ~140–160 bar to ammonium carbamate, which dehydrates to urea and water; unconverted carbamate is decomposed and recycled; the solution is concentrated and prilled or granulated. Biuret forms when urea is heated too long and is harmful to some crops.
Why. Carbamate formation is fast and exothermic; dehydration to urea is slow and equilibrium-limited, so recycle is essential.
How.
- Stripping processes (CO₂ or NH₃ stripping) recover carbamate efficiently.
- Keep biuret low (Indian FCO limit 1.5 % for fertiliser urea) by short residence time at high temperature.
- India mandates neem-coated urea (since 2015) to reduce diversion and slow nitrogen release.
What is the steam-to-carbon ratio in a reformer and why is it important?
Answer. Moles of steam per mole of carbon in the hydrocarbon feed (typically ~2.5–3.5); too low a ratio causes carbon deposition on the nickel catalyst.
Why. Reactions like CH₄ → C + 2H₂ and 2CO → C + CO₂ form coke when steam is short; excess steam shifts equilibrium away from carbon.
How.
- Interlocks trip feed on low steam flow.
- Higher S/C costs energy (more steam), so plants optimise it.
- Tube-skin temperatures and pressure drop show coking.
How is methanol produced?
Answer. From syngas (CO, CO₂, H₂) over Cu/ZnO/Al₂O₃ catalyst at ~50–100 bar and 220–280 °C, followed by distillation.
Why. Exothermic, equilibrium-limited reaction: low temperature favours conversion but the catalyst needs ~250 °C for rate; per-pass conversion is modest, so the gas is recycled.
How.
- CO + 2H₂ ⇌ CH₃OH; CO₂ + 3H₂ ⇌ CH₃OH + H₂O.
- Isothermal (steam-raising) reactors remove heat.
- Purge keeps inerts low.
How is nitric acid made?
Answer. Ostwald process: ammonia is oxidised with air over platinum–rhodium gauze at ~850–900 °C to NO, which is oxidised to NO₂ and absorbed in water to give nitric acid.
Why. Very short contact on Pt–Rh favours NO over N₂; NO₂ absorption needs cooling and pressure.
How.
- 4NH₃ + 5O₂ → 4NO + 6H₂O.
- 2NO + O₂ → 2NO₂; 3NO₂ + H₂O → 2HNO₃ + NO.
- Tail-gas treatment for NOx and N₂O.
Why is CO₂ removed before ammonia synthesis, and where does it go?
Answer. CO₂ (and CO) are oxygen compounds that poison the iron synthesis catalyst and would form ammonium carbamate in the loop; the recovered CO₂ is the raw material for urea.
Why. Oxygen compounds oxidise the active iron surface.
How.
- Hot potassium carbonate (Benfield) or activated MDEA absorption.
- Methanation converts traces to methane (inert, purged).
What is green hydrogen and why is it discussed in energy interviews?
Answer. Hydrogen made by water electrolysis using renewable electricity, with near-zero CO₂ emissions. India’s National Green Hydrogen Mission (2023) targets about 5 million tonnes a year by 2030.
Why. Refineries and fertiliser plants are the largest hydrogen users; today’s grey hydrogen from steam reforming emits ~9–10 kg CO₂ per kg H₂.
How.
- Electrolysers: alkaline, PEM, solid oxide (~50–55 kWh/kg H₂).
- Uses: refinery hydrotreating, green ammonia, methanol, steel.
- Challenges: cost of electricity, storage and transport.
What is the difference between prilling and granulation of urea?
Answer. Prilling sprays molten urea from the top of a tall tower; droplets solidify as they fall into small prills (~1–2 mm). Granulation grows larger, harder granules (2–4 mm) by spraying urea onto recycled seed particles in a fluid bed.
Why. Granules are stronger, less dusty and better for bulk handling and blending; prilling is cheaper but emits dust.
How.
- Prill towers need large air flows and dust scrubbers.
- Granulators use fluidised beds with formaldehyde additive for hardness.
Organisation names show where a topic is a likely focus because of what the organisation does; they are not claims that a particular question was asked. Recruitment routes change each year, so confirm in the official notification.