Metals, alloys and heat treatment
Topics: Properties of materials; ferrous metals: iron–carbon diagram, steels and cast irons; non-ferrous alloys; heat treatment: annealing, normalising, hardening, tempering, surface hardening; testing of materials; plastics and composites.
Properties and testing
Mechanical properties: strength, hardness, toughness, ductility, brittleness, fatigue and creep resistance. The tensile test gives yield strength, ultimate tensile strength (P_max/A₀) and percentage elongation (ductility). Hardness tests: Brinell (ball), Rockwell (quick, depth), Vickers (diamond pyramid). Impact tests (Izod, Charpy) measure toughness.
- UTS = P_max/A₀
- % elongation = (L_f − L₀)/L₀ × 100
- Brinell, Rockwell, Vickers
Example: A 10 mm bar breaks at 50 kN maximum load. Find the UTS.
- A₀ = π × 5² ≈ 78.5 mm².
- UTS = 50 000/78.5 ≈ 637 MPa.
Answer: ≈ 637 MPa
Example: A 50 mm gauge length stretches to 62 mm. Find the percentage elongation.
- (62 − 50)/50 × 100.
- = 24 %.
Answer: 24 %
Iron–carbon diagram
Steel contains up to about 2.1 % carbon, cast iron 2.1–6.67 %. At 727 °C austenite of 0.8 % C (eutectoid) turns into pearlite (ferrite + cementite). Hypo-eutectoid steels (< 0.8 % C) have ferrite plus pearlite; hyper-eutectoid steels have cementite plus pearlite. The lever rule gives the fraction of each phase.
Cast irons: grey (graphite flakes, good damping), white (hard, brittle), malleable and spheroidal-graphite (ductile).
- Eutectoid 0.8 % C, 727 °C
- Steel up to ≈ 2.1 % C
- Lever rule for fractions
Example: A 0.4 % C steel is cooled slowly below 727 °C. Estimate the fraction of pearlite (ferrite holds 0.02 % C).
- Pearlite fraction = (0.4 − 0.02)/(0.8 − 0.02).
- ≈ 0.49 (about half).
Answer: ≈ 49 %
Heat treatment and alloys
Annealing (slow furnace cooling) softens and relieves stress; normalising (air cooling) refines grain; hardening (quenching from austenite) forms hard, brittle martensite; tempering reheats it to restore toughness. Surface hardening: carburising, nitriding, cyaniding, flame and induction hardening give a hard case on a tough core.
Non-ferrous alloys: brass (Cu + Zn), bronze (Cu + Sn), duralumin (Al + Cu + Mg + Mn), gun metal (Cu + Sn + Zn). Stainless steel contains at least about 10.5 % chromium.
- Anneal: soften; normalise: refine grain
- Harden by quench; temper for toughness
- Brass Cu–Zn; bronze Cu–Sn
Example: Why is a hardened chisel tempered?
- Quenching leaves brittle martensite that could chip or shatter.
- Tempering trades a little hardness for toughness.
Answer: To restore toughness
Example: Which alloy is copper with tin?
- Brass is copper with zinc.
- Bronze.
Answer: Bronze
Steels contain up to about 2.1% carbon and cast irons beyond that. On the iron–carbon diagram the eutectoid is at 0.8% C, 723 °C (austenite → pearlite) and the eutectic at 4.3% C, 1147 °C. Annealing softens metal by slow furnace cooling, normalising refines grain by air cooling, hardening quenches to form martensite, and tempering reduces the resulting brittleness. Case hardening (carburising, nitriding) gives a hard surface and a tough core. Brass is copper with zinc, bronze copper with tin. Hardness is tested by Brinell, Rockwell and Vickers, and toughness by Izod and Charpy impact tests.
- Cementite (Fe₃C) is hard and brittle; ferrite is soft.
- Stainless steel has at least about 10.5% Cr, commonly 18-8 (Cr–Ni).
- Duralumin is Al with Cu, Mg, Mn.
- Malleable iron from white cast iron by annealing; grey iron has graphite flakes.
- Ductility is ability to be drawn; malleability to be hammered into sheets.
Key formulas
- Eutectoid: 0.8% C, 723 °C
- Eutectic: 4.3% C, 1147 °C
- BHN = 2P/[πD(D − √(D² − d²))]
Practice questions
Eutectoid carbon content of steel is about
- 0.08%
- 0.8%
- 2.1%
- 4.3%
Show the answer
Answer: B. 0.8% At 723 °C.
Martensite is formed by
- slow cooling
- quenching
- air cooling
- tempering
Show the answer
Answer: B. quenching Rapid cooling.
Tempering is done after
- annealing
- hardening
- casting
- forging only
Show the answer
Answer: B. hardening Reduces brittleness.
Brass is an alloy of copper and
- tin
- zinc
- lead
- aluminium
Show the answer
Answer: B. zinc Bronze has tin.
Bronze is an alloy of copper and
- tin
- zinc
- iron
- magnesium
Show the answer
Answer: A. tin Tin bronze.
Stainless steel owes its corrosion resistance mainly to
- carbon
- chromium
- lead
- sulphur
Show the answer
Answer: B. chromium Passive oxide film.
Impact strength is measured by
- the Izod test
- the Brinell test
- the Rockwell test
- the tensile test only
Show the answer
Answer: A. the Izod test Izod and Charpy.
Grey cast iron contains carbon as
- flakes of graphite
- cementite only
- spheres
- gas
Show the answer
Answer: A. flakes of graphite Flake graphite.
Normalising cools steel in
- the furnace
- still air
- water
- oil
Show the answer
Answer: B. still air Air cooling.
Nitriding produces
- a hard surface
- a soft surface
- a brittle core
- grey iron
Show the answer
Answer: A. a hard surface Surface hardening.
“Bog iron”, used to remove H₂S from coke-oven gas, is
- an intimate mixture of saw dust and iron dust (i.e. moist ferric hydroxide).
- iron impregnated with resin (usually bakelite).
- carbon free iron.
- none of these.
Show the answer
Answer: A. an intimate mixture of saw dust and iron dust (i.e. moist ferric hydroxide).
Iron containing up to about 2 % carbon is called
- pig iron
- wrought iron
- low carbon steel
- none of these
Show the answer
Answer: D. none of these
The softest mineral on Mohs’ scale is
- talc
- gypsum
- rubber
- none of these
Show the answer
Answer: A. talc
Karbate is
- a mixture of iron dust and saw dust.
- carbon impregnated with resin (usually bakelite).
- an acid resistant material.
- both (b) and (c).
Show the answer
Answer: D. both (b) and (c).
Duralumin is an alloy of
- aluminium, copper and manganese.
- aluminium, nickel and silicon.
- aluminium and nickel.
- none of these.
Show the answer
Answer: A. aluminium, copper and manganese.
The corrosion resistance of steel is improved by adding
- phosphorous and tungsten.
- nickel and chromium.
- lead and vanadium.
- molybdenum and tungsten.
Show the answer
Answer: B. nickel and chromium.
White metal is an alloy of
- lead, tin and cadmium
- copper, tin and zinc
- copper and lead
- none of these
Show the answer
Answer: A. lead, tin and cadmium
Adding cobalt to steel improves its
- cutting ability
- corrosion resistance
- tensile strength
- none of these
Show the answer
Answer: A. cutting ability
Pig iron tapped from a blast furnace contains about ____ % carbon.
- 0.2
- 2
- 4
- 8
Show the answer
Answer: C. 4
The carbon content of steel lies in the range of about ____ %.
- 0.1-2
- 4-6
- 2-4
- 0.001-0.01
Show the answer
Answer: A. 0.1-2
A very suitable material for storing 50 % caustic soda solution is
- karbate
- high silicon cast iron
- monel
- none of these
Show the answer
Answer: C. monel
A 15 % brine solution can be stored in a vessel of
- monel
- karbate
- cast iron
- none of these
Show the answer
Answer: A. monel
Concentrated nitric acid is best stored in
- cast iron
- monel
- karbate
- aluminium or chromium alloys (Cr >18% for cold acid)
Show the answer
Answer: D. aluminium or chromium alloys (Cr >18% for cold acid)
Babbitt metal for bearings consists mainly of
- mainly tin (85%) and lead.
- saw dust and iron dust mixture.
- zinc and aluminium.
- copper and aluminium.
Show the answer
Answer: A. mainly tin (85%) and lead.
The rollers of mills that squeeze juice from sugar cane are made of
- stainless steel
- cast iron
- mild steel
- monel
Show the answer
Answer: B. cast iron
The photochemical reactor for chlorinating benzene to BHC is lined with
- karbate
- lead or glass
- fireclay bricks
- PVC
Show the answer
Answer: B. lead or glass
The polymerisation reactor for SBR rubber is made of
- cast iron
- stainless steel or glass lined vessel
- karbate
- wrought iron
Show the answer
Answer: B. stainless steel or glass lined vessel
Evaporators and their tubes for concentrating NaOH to about 70 % are made of
- Cast iron
- Steel
- Nickel
- Karbate
Show the answer
Answer: C. Nickel
Type 316 stainless steel contains approximately
- 16–18 % Cr, 10–14 % Ni and 2–3 % Mo
- 20–22 % Cr and 8–10 % Ni
- 2–4 % Cr, 22 % Ni and 2–4 % Mo
- none of these
Show the answer
Answer: A. 16–18 % Cr, 10–14 % Ni and 2–3 % Mo
Caustic soda can be stored in ____ drums.
- steel
- cast iron
- brass
- gun metal
Show the answer
Answer: A. steel
Brass is an alloy of
- nickel and tin
- copper and zinc
- tin and lead
- copper, nickel and zinc
Show the answer
Answer: B. copper and zinc
The carbonating tower of the Solvay process is made of
- cast iron
- stainless steel
- karbate
- lead lined steel
Show the answer
Answer: A. cast iron
Gun metal is an alloy of
- nickel, tin and copper
- copper, tin and zinc
- copper, phosphorus and nickel
- manganese, phosphorus and nickel
Show the answer
Answer: B. copper, tin and zinc
The balls of a ball mill are usually made of
- steel
- cast iron
- stainless steel
- bronze
Show the answer
Answer: A. steel
Bronze is an alloy of copper with
- lead
- tin
- nickel
- zinc
Show the answer
Answer: B. tin
Rotary cement kilns are lined with
- fireclay
- silica
- lead
- high alumina & high magnesia
Show the answer
Answer: D. high alumina & high magnesia
In the kraft pulping process, the digester is commonly made of
- cast iron
- stainless steel
- karbate carbon
- wrought iron
Show the answer
Answer: A. cast iron
Dry chlorine can be handled in vessels of
- iron or steel
- PVC
- nickel
- brass
Show the answer
Answer: A. iron or steel
A glass-melting tank furnace is built of
- mild steel
- cast iron
- refractory blocks
- stainless steel
Show the answer
Answer: C. refractory blocks
Stainless steel contains
- chromium and nickel
- copper
- aluminium
- vanadium
Show the answer
Answer: A. chromium and nickel
In a mercury cell for caustic soda, the anode and cathode are respectively
- moving mercury and graphite.
- graphite and moving mercury.
- moving mercury and carbon.
- moving mercury and crimped steel wire.
Show the answer
Answer: B. graphite and moving mercury.
Monel metal is an alloy of
- molybdenum and nickel.
- nickel and copper.
- molybdenum and aluminium,
- molybdenum and zinc.
Show the answer
Answer: B. nickel and copper.
German silver is an alloy of
- copper, nickel and zinc.
- copper, aluminium and silver.
- silver, zinc and aluminium.
- silver, nickel and zinc.
Show the answer
Answer: A. copper, nickel and zinc.
Nichrome (chromel) is an alloy of
- chromium and molybdenum.
- nickel and chromium.
- molybdenum and nickel.
- chromium and aluminium.
Show the answer
Answer: B. nickel and chromium.
A material lacking toughness is called
- plastic
- malleable
- brittle
- ductile
Show the answer
Answer: C. brittle
Materials that break at small strains are brittle; those that deform considerably before breaking are
- rigid
- tough
- ductile
- plastic
Show the answer
Answer: C. ductile
Removing the scale formed on steel during hot rolling by acid treatment is called
- descaling
- shot blasting
- pickling
- skimming
Show the answer
Answer: C. pickling
Which joining method gives the weakest joint?
- soldering
- welding
- brazing
- rivetting
Show the answer
Answer: A. soldering
As the carbon content of steel rises, its
- yield stress decreases.
- elongation percent increases.
- tensile strength increases.
- impact strength increases.
Show the answer
Answer: C. tensile strength increases.
The tensile strength of common plastics lies roughly between ____ kg/mm².
- 10 to 50
- 50 to 100
- 0.01 to 0.1
- 0.1 to 10
Show the answer
Answer: D. 0.1 to 10
Which of these abrasives is synthetic?
- Corundum
- Emery
- Pumice
- Silicon caride
Show the answer
Answer: D. Silicon caride
Which of these is NOT ferromagnetic?
- Nickel
- Cobalt
- Aluminium
- Iron
Show the answer
Answer: C. Aluminium
Young’s modulus measures a material’s
- stiffness
- malleability
- creep resistance
- tensile strength
Show the answer
Answer: A. stiffness
Whether a material is ductile or brittle is best judged by the ____ test.
- Impact
- Cupping
- Hardness
- Tensile
Show the answer
Answer: A. Impact
For steel to respond to hardening treatment, its carbon content should be at least about ____ %.
- 0.2
- 0.4
- 0.6
- 0.8
Show the answer
Answer: A. 0.2
Photographic plates are coated with
- silver nitrate
- silver halide
- calcium silicats
- metallic silver
Show the answer
Answer: B. silver halide
Power-saw blades are made of
- Wrought iron
- Stainless steel
- Mild steel
- High speed steel
Show the answer
Answer: D. High speed steel
Which welding process reaches the highest temperature?
- Arc welding
- Gas welding
- Thermit welding
- Resistance welding
Show the answer
Answer: A. Arc welding
In brazing, metals are joined
- without melting the base metal.
- by melting the base metal.
- at temperatures above 450°C.
- none of these.
Show the answer
Answer: A. without melting the base metal.
A metal weighs 5 kg in air and 4 kg in water. Its specific gravity is
- 5
- 1.25
- 2.5
- 3.75
Show the answer
Answer: A. 5
The Rockwell number indicates
- hardness of a substance.
- colour of a pigment.
- density of a polymer.
- active ingredients in a fertiliser.
Show the answer
Answer: A. hardness of a substance.
Which metal reacts violently with water?
- Mercury
- Sodium
- Calcium
- Magnesium
Show the answer
Answer: B. Sodium
Lubrication is used to control
- friction
- wear
- temperature
- all (a), (b) & (c)
Show the answer
Answer: D. all (a), (b) & (c)
A material that expands freely on heating develops
- no
- compressive
- tensile
- thermal
Show the answer
Answer: A. no
The flux most used for brazing is
- zinc chloride
- borax
- ammonium chloride
- rosin
Show the answer
Answer: B. borax
Work-hardening steel for excavator buckets and bulldozer blades contains iron, carbon and
- manganese
- silicon
- nickel
- chromium
Show the answer
Answer: A. manganese
The cobalt–chromium–tungsten cast alloy used for cutting tools is
- Stellite
- High speed steel
- Cermet
- Alnico
Show the answer
Answer: A. Stellite
The most wear-resistant carbide for cutting tools is
- Aluminium carbide
- Tungsten carbide
- Nickel carbide
- Iron carbide
Show the answer
Answer: B. Tungsten carbide
Twist drills are usually made of
- cermets
- high speed steel
- alloy steel
- tungsten carbide
Show the answer
Answer: B. high speed steel
Adding which elements increases the hardness of carbon tool steel?
- vanadium & chromium
- silicon
- tungsten
- manganese
Show the answer
Answer: A. vanadium & chromium
Ceramic cutting-tool tips are made from
- carbon
- silicon carbide
- aluminium oxide
- tungsten
Show the answer
Answer: C. aluminium oxide
Electrochemical corrosion needs a ____ in contact with the metal.
- air
- oxygen
- liquid medium
- gaseous medium
Show the answer
Answer: C. liquid medium
Which lubricants have the least oiliness?
- Mineral oils
- Vegetable oils
- Greases
- Animal oils
Show the answer
Answer: A. Mineral oils
For a machine working at high temperature and load, the best lubricant is a
- grease
- solid lubricant
- animal oils
- mineral oils
Show the answer
Answer: B. solid lubricant
Automobile catalytic converters use a ____ catalyst.
- alumina
- platinum
- vanadium pentoxide
- iron oxide
Show the answer
Answer: B. platinum
The low-melting bismuth–lead alloy used for fuses is
- Wood's metal
- Babbit metal
- Monel metal
- Duralumin
Show the answer
Answer: A. Wood's metal
Holes for riveted joints are best made by
- drilling
- tapping
- reaming
- punching
Show the answer
Answer: A. drilling
For a riveted joint, if plate thickness is made four times larger, the rivet diameter should be made about ____ times larger.
- two
- four
- six
- eight
Show the answer
Answer: A. two
Iron loses its ferromagnetism at the Curie point, about ____ °C.
- 768
- 908
- 1400
- 1539
Show the answer
Answer: A. 768
Which material shows a distinct yield point?
- hard bronze
- soft brass
- cold rolled mild steel
- hot rolled mild steel
Show the answer
Answer: D. hot rolled mild steel
Steels commonly contain chromium up to about ____ %.
- 12
- 18
- 24
- 30
Show the answer
Answer: B. 18
The maximum permissible sulphur in steel is about ____ %.
- 0.015
- 0.055
- 0.505
- 0.805
Show the answer
Answer: B. 0.055
Which of these is the most malleable?
- Lead
- Copper
- Aluminium
- Wrought iron
Show the answer
Answer: A. Lead
Which element controls the properties of steel most?
- Manganese
- Silicon
- Carbon
- Vanadium
Show the answer
Answer: C. Carbon
Which addition increases the depth of hardening of steel?
- Chromium
- Nickel
- Tungsten
- Vanadium
Show the answer
Answer: A. Chromium
Fatigue resistance is measured by the
- elastic limit.
- ultimate tensile strength.
- Young's modulus.
- endurance limit.
Show the answer
Answer: D. endurance limit.
As impurities in a metal increase, its corrosion resistance
- increase
- decrease
- remain same
- may increase or decrease; depending on the type of metal
Show the answer
Answer: D. may increase or decrease; depending on the type of metal
Dezincification is corrosion of
- steel
- brass
- stainless steel
- babbit metal
Show the answer
Answer: B. brass
Cermets are usually about 80 % ceramic and 20 % metal. Which of these is a cermet?
- Zirconia
- Alumina
- Bakelite
- Tungsten carbide
Show the answer
Answer: D. Tungsten carbide
Foundry crucibles are made of
- lead
- stainless steel
- graphite
- cast iron
Show the answer
Answer: C. graphite
Dezincification mainly attacks
- brass
- nichrome
- stainless steel
- monel
Show the answer
Answer: A. brass
A fibrous fracture surface is typical of ____ materials.
- hard
- elastic
- ductile
- brittle
Show the answer
Answer: C. ductile
Which treatment does NOT protect a metal from corrosion?
- tempering
- chromising
- aluminising
- alloying
Show the answer
Answer: A. tempering
Silicon steel for electrical machines contains about ____ % silicon.
- 0.3-0.4
- 12-14
- 3-4
- 20-25
Show the answer
Answer: C. 3-4
Cold chisels and hammers are made of
- high speed steel
- high carbon steel
- forged steel
- mild steel
Show the answer
Answer: B. high carbon steel
Steel is heat-treated mainly to change its
- mechanical properties.
- physical properties.
- chemical composition.
- all a, b & c.
Show the answer
Answer: A. mechanical properties.
Coating steel with aluminium for resistance to oxidation up to about 700 °C is called
- Vaneering
- Galvanising
- Electroplating
- Calorising
Show the answer
Answer: D. Calorising
Cast iron water mains are usually joined by ____ joints.
- Collar
- Flanged
- Bell and Spigot
- Expansion
Show the answer
Answer: C. Bell and Spigot
Which of these is NOT a metalloid?
- Arsenic
- Antimony
- Lead
- none of these
Show the answer
Answer: C. Lead
The ultimate shear strength of steel is roughly ____ times its ultimate tensile strength.
- 0.5
- 0.75
- 1.5
- 2.5
Show the answer
Answer: B. 0.75
Which material has a negative coefficient of linear expansion when stretched?
- Iron
- Copper
- Rubber
- Nickel
Show the answer
Answer: C. Rubber
Factor of safety for ductile materials is the ratio of ____ stress to working stress.
- tensile
- compressive
- yield
- bearing
Show the answer
Answer: C. yield
The practice questions were written for this studio; they are not copied from ASTU papers. ASTU publishes no topic syllabus for these exams, so the topics are an informed guide based on diploma courses, not an official list.