PVC is the third most-produced plastic. Its monomer, vinyl chloride (VCM), is made by the balanced process: ethylene is chlorinated directly and by oxychlorination to ethylene dichloride (EDC), EDC is cracked to VCM and HCl, and the HCl is recycled to oxychlorination so there is no net HCl. About 80 % of PVC is made by suspension polymerisation: VCM droplets dispersed in water with a suspending agent are polymerised with an oil-soluble initiator in batch reactors; the porous grains are stripped of residual VCM, centrifuged and dried.

Raw materials

  • Ethylene and chlorine (from chlor-alkali), oxygen/air
  • Catalysts: FeCl₃ (direct chlorination), CuCl₂ on alumina (oxychlorination)
  • Polymerisation: demineralised water, suspending agents (PVA, cellulose ethers), initiators (peroxydicarbonates, lauroyl peroxide)
  • Additives at compounding: plasticisers (DOP/DINP), heat stabilisers, lubricants, fillers

Products

  • Suspension PVC resin (K-value 57–70)
  • Emulsion/paste PVC for coatings and leather cloth
  • Rigid (uPVC) and flexible (plasticised) compounds

Uses

  • Pipes and fittings (≈ 70 % in India), window profiles
  • Cables, flooring, films, leather cloth, footwear
  • Medical tubing and bags

Reactions

  • Direct chlorination: C₂H₄ + Cl₂ → C₂H₄Cl₂ (EDC) FeCl₃, 50–70 °C
  • Oxychlorination: C₂H₄ + 2HCl + ½O₂ → C₂H₄Cl₂ + H₂O CuCl₂, 220–300 °C
  • EDC cracking: C₂H₄Cl₂ → CH₂=CHCl + HCl 480–520 °C, 20–30 bar
  • Polymerisation: n CH₂=CHCl → –(CH₂–CHCl)ₙ– ΔH ≈ −96 kJ/mol

Operating conditions

EDC cracking480–520 °C, 50–60 % conversion per pass
Suspension reactor50–70 °C (sets K-value), 8–12 bar, 4–8 h batch, 30–200 m³
ConversionStopped at 85–90 % (pressure drop)
VCM strippingSteam stripping column; residual VCM < 1 ppm in resin
DryingFluid-bed / flash dryer to < 0.3 % moisture

Process, step by step

  1. EDC production. Ethylene reacts with chlorine in liquid EDC (direct chlorination, FeCl₃) and, in parallel, with recycled HCl and oxygen over copper chloride catalyst (oxychlorination). EDC from both is washed and purified by distillation.
  2. EDC cracking and VCM purification. Pure EDC is cracked in a fired furnace at 480–520 °C. The gas is quenched; HCl is distilled off and recycled to oxychlorination, VCM is distilled overhead, and unconverted EDC is recycled to purification.
  3. Reactor charging. Demineralised water, suspending agents and buffer are charged to a jacketed, agitated, stainless-steel or glass-lined reactor; air is removed, VCM is charged, and the initiator is added. Agitation disperses VCM into droplets of 30–150 µm.
  4. Suspension polymerisation. At 50–70 °C (temperature sets molecular weight/K-value) polymer forms inside each droplet, which becomes a porous PVC grain. Heat is removed by the jacket and reflux condenser. When the pressure falls (VCM consumed, ≈ 85–90 % conversion) the reaction is stopped with a short-stop.
  5. VCM recovery and stripping. Unreacted VCM is vented to a gas holder and recovered by compression and condensation. The slurry is steam-stripped in a column to reduce residual VCM in the resin to below 1 ppm — essential because VCM is a carcinogen.
  6. Dewatering and drying. Slurry is dewatered in decanter centrifuges and dried in fluid-bed or cyclone dryers, sieved and stored in silos; the resin is compounded with stabilisers and plasticisers by the processors.

Major engineering problems

VCM toxicity (angiosarcoma of the liver)

Closed-reactor technology, reactor cleaning without entry (anti-fouling coatings, high-pressure jets), stripping to < 1 ppm, workplace monitoring.

Heat removal and fouling

Jacket + reflux condensers, anti-scale coatings, controlled initiator activity.

Dioxins and chlorinated by-products

Incineration of heavy ends with HCl recovery, good oxychlorination control.

Corrosion by HCl

Dry systems, nickel alloys, careful moisture control.

Thermal instability of PVC

Heat stabilisers (Ca–Zn, organotin; lead phased out).

Notes

  • K-value (Fikentscher) indicates molecular weight: 57 for bottles, 65–67 for pipes, 70 for cables.
  • PVC contains 57 % chlorine by mass — less dependent on oil than other plastics.
  • Emulsion PVC uses water-soluble persulphate initiator and gives fine paste resin.

Practice questions

VCM is obtained by cracking

  1. ethylene
  2. ethylene dichloride
  3. vinyl acetate
  4. acetylene
Show the answer

Answer: B. ethylene dichloride EDC → VCM + HCl.

In the balanced process, HCl from EDC cracking is

  1. sold
  2. recycled to oxychlorination
  3. neutralised
  4. vented
Show the answer

Answer: B. recycled to oxychlorination No net HCl.

Most PVC is made by

  1. bulk
  2. suspension
  3. emulsion
  4. gas-phase
Show the answer

Answer: B. suspension ≈ 80 %.

The polymerisation temperature of PVC mainly controls its

  1. colour
  2. K-value (molecular weight)
  3. density
  4. chlorine content
Show the answer

Answer: B. K-value (molecular weight) Lower T → higher K.

Residual VCM in PVC resin must be kept below about

  1. 1 %
  2. 1000 ppm
  3. 1 ppm
  4. 50 %
Show the answer

Answer: C. 1 ppm Carcinogen.

The oxychlorination catalyst is

  1. FeCl₃
  2. CuCl₂
  3. V₂O₅
  4. Ni
Show the answer

Answer: B. CuCl₂ On alumina, 220–300 °C.

Theory questions

Describe the manufacture of PVC by suspension polymerisation, including VCM production. (10 marks)

Show the model answer

Direct chlorination (FeCl₃) and oxychlorination (CuCl₂) of ethylene to EDC; purification; cracking at 500 °C; HCl column (recycle), VCM column; batch suspension reactor with water, PVA, initiator, 50–70 °C, 8–12 bar, stop at 85–90 %; VCM recovery; steam stripping; centrifuge; fluid-bed drying; silos.

Why is the balanced VCM process used? (3 marks)

Show the model answer

Cracking EDC gives one mole HCl per mole VCM; using this HCl in oxychlorination to make more EDC consumes it completely, so only ethylene, chlorine and oxygen are required and no HCl by-product needs disposal.

Frequently asked questions

How is polyvinyl chloride (pvc) manufactured?

Balanced VCM process + suspension polymerisation. PVC is the third most-produced plastic. Its monomer, vinyl chloride (VCM), is made by the balanced process: ethylene is chlorinated directly and by oxychlorination to ethylene dichloride (EDC), EDC is cracked to VCM and HCl, and the HCl is recycled to oxychlorination so there is no net HCl. About 80 % of PVC is made by suspension polymerisation: VCM droplets dispersed in water with a suspending agent are polymerised with an oil-soluble initiator in batch reactors; the porous grains are stripped of residual VCM, centrifuged and dried.

What raw materials are used to make polyvinyl chloride (pvc)?

Ethylene and chlorine (from chlor-alkali), oxygen/air; Catalysts: FeCl₃ (direct chlorination), CuCl₂ on alumina (oxychlorination); Polymerisation: demineralised water, suspending agents (PVA, cellulose ethers), initiators (peroxydicarbonates, lauroyl peroxide); Additives at compounding: plasticisers (DOP/DINP), heat stabilisers, lubricants, fillers

What catalyst is used in polyvinyl chloride (pvc) production?

organic peroxide initiators (suspension); CuCl₂ for oxychlorination

What is polyvinyl chloride (pvc) used for?

Pipes and fittings (≈ 70 % in India), window profiles; Cables, flooring, films, leather cloth, footwear; Medical tubing and bags

Watch the animated P&ID →