IITIAN1997 STUDIO

Polyethylene (LLDPE and HDPE)

Gas-phase fluidised-bed (Unipol) and slurry-loop processes

Watch the animated P&ID →

Polyethylene is the world’s largest-volume plastic. High-density polyethylene (HDPE) is a nearly linear polymer made at low pressure with Ziegler–Natta or Phillips chromium catalysts; linear low-density polyethylene (LLDPE) is a copolymer of ethylene with a few per cent of 1-butene, 1-hexene or 1-octene, whose short branches lower crystallinity and density. Both are produced in gas-phase fluidised-bed reactors (Unipol type) or slurry processes. (LDPE, the branched polymer, needs free-radical polymerisation at 1500–3000 bar.)

Raw materials

  • Polymer-grade ethylene (99.95 %)
  • Comonomer: 1-butene, 1-hexene, 1-octene (LLDPE and HDPE grades)
  • Catalyst: Ziegler–Natta (TiCl₄/MgCl₂ + triethylaluminium co-catalyst), Phillips (CrO₃/SiO₂), metallocene
  • Hydrogen (molecular-weight control), isobutane/hexane diluent (slurry), nitrogen

Products

  • HDPE (density 0.941–0.965 g/cm³) — pipes, blow-moulded containers, crates
  • LLDPE (0.915–0.940) — stretch and packaging film
  • LDPE (0.910–0.925) — film, coating, cable insulation

Uses

  • Packaging film, carry bags, milk pouches
  • Pipes (PE-100), water tanks, drums, crates
  • Wire and cable insulation, rotomoulding, toys

Reactions

  • Coordination polymerisation: n CH₂=CH₂ → –(CH₂–CH₂)ₙ– ΔH ≈ −93 kJ/mol (very exothermic)
  • Copolymerisation: CH₂=CH₂ + CH₂=CH–C₂H₅ → short ethyl branches (LLDPE)
  • Chain transfer by H₂: controls melt flow index (MFI)
  • Cossee mechanism: monomer insertion into Ti–C bond

Operating conditions

Gas-phase (LLDPE/HDPE)80–110 °C, 20–25 bar, single-pass conversion 2–5 %, overall > 98 %
Slurry loop (HDPE)70–110 °C, 30–40 bar, isobutane diluent, Phillips/Ziegler
LDPE (for comparison)1500–3000 bar, 200–300 °C, peroxide/O₂ initiator, tubular or autoclave
Catalyst productivity10–50 kg PE per g catalyst (no removal needed)
Product controlMFI via H₂/C₂H₄ ratio; density via comonomer/C₂H₄ ratio

Process, step by step

  1. Feed purification. Ethylene, comonomer, hydrogen and nitrogen are purified over copper, alumina and molecular-sieve beds to remove ppm-level poisons (O₂, H₂O, CO, CO₂, acetylene, sulphur) that would deactivate the highly sensitive catalyst.
  2. Catalyst feeding. Dry catalyst powder (or slurry) is injected into the reactor bed with a nitrogen carrier; the co-catalyst (triethylaluminium) is fed separately.
  3. Fluidised-bed polymerisation. Cycle gas (ethylene, comonomer, H₂, N₂) enters through a distributor plate and fluidises a bed of growing polymer particles. Polymer forms on each catalyst particle, which grows to 0.5–1.5 mm. Only 2–5 % of the ethylene reacts per pass; the expanded top section lets particles disengage from the gas.
  4. Cycle-gas cooling. The heat of polymerisation is removed by circulating large volumes of gas through a compressor and cooler. In "condensed mode" part of the cycle gas (with an inert condensing agent such as isopentane) is condensed and evaporates in the bed, greatly raising capacity.
  5. Product discharge and degassing. Polymer powder is removed intermittently through a product discharge system into a purge bin, where nitrogen (and steam) strips dissolved hydrocarbons and deactivates residual catalyst; vent gas is recovered.
  6. Extrusion and pelletising. Powder is mixed with additives (antioxidants, slip/antiblock agents, stabilisers) and melted in a twin-screw extruder, then cut by an underwater pelletiser, dried, blended in silos and bagged.

Major engineering problems

Large heat of reaction

High cycle-gas flow, condensed-mode operation, loop reactors with jacket cooling (slurry).

Catalyst poisoning

Deep feed purification to ppb levels.

Sheeting/agglomeration and static in fluid beds

Static control agents, temperature control below polymer sticking point, good fluidisation.

Grade transitions and off-spec

Model-based control of H₂/C₂ and comonomer ratios; minimise transition time.

Hydrocarbon emissions

Vent recovery by compression/condensation/membranes, flare.

Notes

  • Ziegler (1953) and Natta received the 1963 Nobel prize for coordination catalysts.
  • Melt flow index (190 °C, 2.16 kg) indicates molecular weight — film grades MFI ≈ 1, injection grades 5–20.
  • Bimodal HDPE (two reactors in series) gives strong, crack-resistant pipe grades.

Practice questions

LLDPE is a copolymer of ethylene with

  1. propylene
  2. α-olefins such as 1-butene or 1-hexene
  3. vinyl chloride
  4. styrene
Show the answer

Answer: B. α-olefins such as 1-butene or 1-hexene Short branches.

HDPE is made with

  1. peroxides at 2000 bar
  2. Ziegler–Natta or Phillips catalysts at low pressure
  3. acid catalysts
  4. enzymes
Show the answer

Answer: B. Ziegler–Natta or Phillips catalysts at low pressure Coordination polymerisation.

LDPE is produced at about

  1. 1–10 bar
  2. 20–40 bar
  3. 1500–3000 bar
  4. vacuum
Show the answer

Answer: C. 1500–3000 bar Free-radical, high pressure.

Molecular weight in Ziegler PE processes is controlled by

  1. nitrogen
  2. hydrogen
  3. oxygen
  4. water
Show the answer

Answer: B. hydrogen Chain transfer agent.

The heat of polymerisation in the Unipol process is removed by

  1. jacket only
  2. cooling the circulating cycle gas
  3. adding water
  4. vacuum
Show the answer

Answer: B. cooling the circulating cycle gas Condensed-mode operation.

Density of HDPE is about

  1. 0.88
  2. 0.92
  3. 0.95–0.96
  4. 1.38
Show the answer

Answer: C. 0.95–0.96 High crystallinity.

Theory questions

Describe the manufacture of LLDPE/HDPE by the gas-phase process. (8 marks)

Show the model answer

Purification of ethylene, comonomer, H₂; catalyst (Ziegler/metallocene) injection; fluidised-bed reactor 80–110 °C, 20–25 bar, 2–5 % per pass; cycle gas compressed and cooled (condensed mode); product discharge, N₂ purge bin; extrusion with additives, underwater pelletising, silos. Density via comonomer ratio, MFI via H₂ ratio.

Compare LDPE, LLDPE and HDPE. (4 marks)

Show the model answer

LDPE: free radical, 1500–3000 bar, long branches, 0.91–0.925, soft film. LLDPE: Ziegler/metallocene copolymer, low pressure, short branches, 0.915–0.94, tough film. HDPE: linear, Ziegler/Phillips, 0.941–0.965, rigid — pipes, containers.

Frequently asked questions

How is polyethylene (lldpe and hdpe) manufactured?

Gas-phase fluidised-bed (Unipol) and slurry-loop processes. Polyethylene is the world’s largest-volume plastic. High-density polyethylene (HDPE) is a nearly linear polymer made at low pressure with Ziegler–Natta or Phillips chromium catalysts; linear low-density polyethylene (LLDPE) is a copolymer of ethylene with a few per cent of 1-butene, 1-hexene or 1-octene, whose short branches lower crystallinity and density. Both are produced in gas-phase fluidised-bed reactors (Unipol type) or slurry processes. (LDPE, the branched polymer, needs free-radical polymerisation at 1500–3000 bar.)

What raw materials are used to make polyethylene (lldpe and hdpe)?

Polymer-grade ethylene (99.95 %); Comonomer: 1-butene, 1-hexene, 1-octene (LLDPE and HDPE grades); Catalyst: Ziegler–Natta (TiCl₄/MgCl₂ + triethylaluminium co-catalyst), Phillips (CrO₃/SiO₂), metallocene; Hydrogen (molecular-weight control), isobutane/hexane diluent (slurry), nitrogen

What catalyst is used in polyethylene (lldpe and hdpe) production?

Ziegler–Natta (TiCl₄/MgCl₂ + AlEt₃) or Phillips chromium

What is polyethylene (lldpe and hdpe) used for?

Packaging film, carry bags, milk pouches; Pipes (PE-100), water tanks, drums, crates; Wire and cable insulation, rotomoulding, toys

Watch the animated P&ID →