On the paper machine a very dilute suspension of fibres (about 0.5–1 % consistency) is spread on a moving wire screen, where water drains and the fibres interlace into a mat. The wet web is then pressed and dried on steam-heated cylinders, smoothed in a calender and wound on a reel. Most of the art lies in stock preparation — refining (beating) the fibres to develop bonding, and adding fillers, sizing and other chemicals that give the paper its opacity, printability and water resistance.
Raw materials
- Bleached or unbleached chemical pulp, mechanical pulp, recycled fibre (deinked)
- Fillers: china clay, precipitated calcium carbonate, TiO₂
- Sizing: rosin + alum (acid) or AKD/ASA (alkaline)
- Retention aids, wet-strength resins, dyes, optical brighteners, starch
Products
- Writing and printing paper, newsprint
- Kraft paper, liner and corrugating medium, paper board
- Tissue and speciality papers
Uses
- Printing and writing papers, newsprint, books and notebooks
- Packaging: cartons, corrugated boxes, paper sacks and bags
- Hygiene and speciality: tissue, filter paper, currency and security paper
Reactions
- Rosin sizing: rosin soap + Al₂(SO₄)₃ → aluminium resinate precipitated on fibres (pH 4.5–5.5)
- AKD (alkyl ketene dimer) reacts with cellulose –OH (neutral/alkaline sizing)
- Precipitated CaCO₃: Ca(OH)₂ + CO₂ → CaCO₃ (on-site PCC plants)
Operating conditions
| Headbox consistency | 0.5–1.0 % |
|---|---|
| After wire | ≈ 18–22 % solids |
| After press section | 40–50 % solids |
| After dryers | 92–95 % solids |
| Machine speed | 300–2000 m/min |
| Basis weight | 40–400 g/m² (GSM) |
Process, step by step
- Stock preparation. Baled or slush pulp is dispersed in water in a pulper. The stock is refined in disc refiners (beating), which fibrillates and hydrates the fibres, raising their bonding area and strength while reducing freeness. Broke (rejected paper) is repulped and returned.
- Blending and additives. In the machine chest, stock from different pulps is blended and fillers, sizing agents, retention aids, dyes and wet-strength resins are added. Proportions decide the grade of paper.
- Approach flow. The thick stock is diluted with white water (water drained from the wire) to 0.5–1 % in the fan pump and cleaned in centrifugal cleaners and pressure screens that remove sand, shives and dirt.
- Forming (wire section). The headbox delivers a uniform jet across the full width onto the moving Fourdrinier wire (or between two wires in gap formers). Water drains through table rolls, foils and suction boxes; fibres mat together into a web of about 20 % solids. Drained white water is recycled.
- Pressing. The web is carried by felts through press nips (including shoe presses) that squeeze out water mechanically to 40–50 % dryness — far cheaper than drying by heat.
- Drying. The web runs over 40–60 steam-heated cast-iron cylinders in the dryer section, held against them by dryer fabrics, until it reaches 92–95 % solids. A size press may apply starch on the surface.
- Calendering and reeling. The dry sheet passes between polished steel rolls of the calender stack to smooth it and control thickness, then is wound on the reel. Rolls are slit and rewound, or cut into sheets, and coated if required.
Major engineering problems
Huge water consumption
Closing the white-water loop, save-alls (fibre recovery), effluent treatment and reuse — modern mills < 20 m³/t.
Energy for drying
Maximise press dewatering (shoe presses), heat recovery from hoods, efficient steam/condensate systems.
Deposits, pitch and slime
Biocides, retention control, cleanliness.
Uniformity of the sheet
Headbox dilution control, scanning QCS gauges (basis weight, moisture, caliper).
Fibre losses and solid waste
Save-alls, sludge dewatering and incineration or use in boards.
Notes
- Consistency = mass of dry fibre / mass of stock × 100.
- Freeness (CSF) measures drainage — refined pulp has lower freeness.
- GSM = grams per square metre.
- Cylinder-mould machines make multi-ply boards; Yankee dryers make tissue.
Practice questions
Consistency of stock at the headbox is about
- 0.5–1 %
- 5 %
- 20 %
- 45 %
Show the answer
Answer: A. 0.5–1 % Very dilute for good formation.
Beating (refining) of pulp
- reduces strength
- fibrillates fibres to increase bonding
- removes lignin
- bleaches pulp
Show the answer
Answer: B. fibrillates fibres to increase bonding Increases bonding area.
Rosin sizing is fixed on fibres with
- NaOH
- alum
- starch
- clay
Show the answer
Answer: B. alum Aluminium resinate.
Most water is removed from the web in the
- dryer section
- wire (forming) section
- calender
- reel
Show the answer
Answer: B. wire (forming) section 0.7 % → 20 % solids.
China clay is added to paper as a
- sizing agent
- filler (opacity, smoothness)
- bleach
- wet-strength resin
Show the answer
Answer: B. filler (opacity, smoothness) Also CaCO₃, TiO₂.
The calender
- dries the sheet
- smooths the sheet and controls thickness
- forms the sheet
- adds size
Show the answer
Answer: B. smooths the sheet and controls thickness Polished steel rolls.
Theory questions
Describe paper making on a Fourdrinier machine. (8 marks)
Show the model answer
Stock preparation (pulping, refining, blending with fillers, size, dyes); dilution with white water to 0.5–1 %; cleaning and screening; headbox; forming on the moving wire with table rolls, foils, suction boxes (to 20 %); press section (40–50 %); steam-heated dryer cylinders (92–95 %); size press; calender; reel; white-water recycle.
Explain the purpose of sizing and fillers. (3 marks)
Show the model answer
Sizing (rosin/alum, AKD, ASA; surface starch) makes paper resistant to water and ink penetration so it can be written on. Fillers (clay, CaCO₃, TiO₂) fill spaces between fibres to improve opacity, brightness, smoothness and printability and reduce cost.
Frequently asked questions
How is paper making manufactured?
Stock preparation and the Fourdrinier paper machine. On the paper machine a very dilute suspension of fibres (about 0.5–1 % consistency) is spread on a moving wire screen, where water drains and the fibres interlace into a mat. The wet web is then pressed and dried on steam-heated cylinders, smoothed in a calender and wound on a reel. Most of the art lies in stock preparation — refining (beating) the fibres to develop bonding, and adding fillers, sizing and other chemicals that give the paper its opacity, printability and water resistance.
What raw materials are used to make paper making?
Bleached or unbleached chemical pulp, mechanical pulp, recycled fibre (deinked); Fillers: china clay, precipitated calcium carbonate, TiO₂; Sizing: rosin + alum (acid) or AKD/ASA (alkaline); Retention aids, wet-strength resins, dyes, optical brighteners, starch
What catalyst is used in paper making production?
no catalyst (mechanical and drying operations)
What is paper making used for?
Printing and writing papers, newsprint, books and notebooks; Packaging: cartons, corrugated boxes, paper sacks and bags; Hygiene and speciality: tissue, filter paper, currency and security paper