IITIAN1997 STUDIO

Synthetic Fibres

Polyester (PET) continuous polymerisation and melt spinning; nylon

Watch the animated P&ID →

Synthetic fibres are long-chain polymers spun into filaments. Polyester (polyethylene terephthalate, PET) is the largest; it is produced by esterifying purified terephthalic acid (PTA) with monoethylene glycol (MEG) and polycondensing the product under high vacuum at 280–290 °C with an antimony catalyst. The molten polymer is spun directly through spinnerets, cooled and drawn to orient the chains and develop strength. Nylon-6,6 is made by polycondensation of nylon salt (adipic acid + hexamethylenediamine), nylon-6 by ring-opening of caprolactam, and acrylic fibres by solution spinning of polyacrylonitrile.

Raw materials

  • PET: purified terephthalic acid (from p-xylene) and monoethylene glycol (from ethylene oxide)
  • Catalysts and additives: Sb₂O₃/antimony acetate, TiO₂ (delustrant), stabilisers
  • Nylon-6,6: adipic acid + hexamethylenediamine; nylon-6: caprolactam
  • Acrylic: acrylonitrile (+ vinyl acetate), solvent DMF/NaSCN

Products

  • Polyester staple fibre (PSF), partially oriented yarn (POY), fully drawn yarn (FDY)
  • Bottle-grade PET chips (after solid-state polymerisation)
  • Nylon filament, tyre cord; acrylic staple

Uses

  • Apparel and home textiles (blends with cotton/viscose)
  • Industrial yarn, tyre cord, ropes, nets
  • PET bottles and films

Reactions

  • Esterification: HOOC–C₆H₄–COOH + 2HOCH₂CH₂OH → BHET + 2H₂O (250–270 °C)
  • Polycondensation: n BHET → PET + n HOCH₂CH₂OH (Sb₂O₃, 280–290 °C, < 1 mbar)
  • Nylon-6,6: n HOOC(CH₂)₄COOH + n H₂N(CH₂)₆NH₂ → nylon-6,6 + 2n H₂O
  • Nylon-6: ring-opening of caprolactam (water-initiated, 250–270 °C)

Operating conditions

Esterification250–270 °C, 1–3 bar, MEG : PTA ≈ 1.1–1.2
Pre-polycondensation260–280 °C, 20–100 mbar
Final polycondensation280–290 °C, < 1 mbar, disc-ring finisher (high viscosity)
Intrinsic viscosityFibre 0.62–0.65 dL/g; bottle 0.75–0.85 (SSP)
SpinningMelt spinning ≈ 290 °C, quench air, take-up 3000–6000 m/min (POY)
DrawingDraw ratio 3–5, 80–180 °C

Process, step by step

  1. Paste preparation. PTA powder and MEG (with catalyst and TiO₂ slurry) are mixed into a paste in an agitated paste mixer and fed continuously to the esterifier.
  2. Esterification. At 250–270 °C and slightly above atmospheric pressure PTA reacts with MEG to form bis-hydroxyethyl terephthalate (BHET) and low oligomers. Water is removed in a column on top that returns MEG to the reactor.
  3. Pre-polycondensation. The oligomer flows to pre-polymerisers under reduced pressure (20–100 mbar) at 260–280 °C, where MEG is released as chains grow to a degree of polymerisation of about 20–30.
  4. Final polycondensation. In the horizontal disc-ring finisher under high vacuum (< 1 mbar) at 280–290 °C, rotating discs create thin films from which MEG evaporates, raising the molecular weight to fibre grade (IV ≈ 0.64). MEG vapour is condensed, purified and recycled.
  5. Melt spinning. The molten polymer is pumped by gear (metering) pumps through filter packs and spinnerets with hundreds of fine holes. Filaments are cooled by cross-flow quench air, given spin finish and wound as POY or collected as tow.
  6. Drawing and finishing. Filaments are drawn 3–5 times over heated godets to orient and crystallise the chains (strength, low elongation), then texturised (yarn) or crimped, heat-set and cut into staple fibre and baled.

Major engineering problems

Removal of MEG at high viscosity

Disc-ring finishers giving large surface renewal, high vacuum.

Degradation (colour, acetaldehyde, DEG)

Short residence, controlled temperature, stabilisers; DEG < 1.5 %.

Spinning breaks and uniformity

Melt filtration, precise metering, controlled quench.

Energy and vacuum systems

Steam-jet/liquid-ring vacuum with glycol ejectors; heat integration (Dowtherm heating).

Microplastics and recycling

Bottle-to-fibre recycling (rPET), chemical recycling (glycolysis).

Notes

  • India’s polyester capacity is among the world’s largest (Reliance, Indorama).
  • Intrinsic viscosity (IV) is a measure of molecular weight for PET.
  • Melt spinning needs a polymer stable above its melting point; acrylics decompose before melting and are solution-spun.

Practice questions

PET is made from

  1. adipic acid + HMDA
  2. terephthalic acid + ethylene glycol
  3. caprolactam
  4. acrylonitrile
Show the answer

Answer: B. terephthalic acid + ethylene glycol PTA + MEG.

The catalyst commonly used in PET polycondensation is

  1. V₂O₅
  2. Sb₂O₃ (antimony)
  3. Ni
  4. AlCl₃
Show the answer

Answer: B. Sb₂O₃ (antimony) Antimony compounds.

Final polycondensation of PET is carried out under

  1. high pressure
  2. high vacuum
  3. nitrogen at 10 bar
  4. atmospheric air
Show the answer

Answer: B. high vacuum To remove MEG.

Acrylic fibres are spun by

  1. melt spinning
  2. solution (wet/dry) spinning
  3. electrospinning only
  4. gel spinning only
Show the answer

Answer: B. solution (wet/dry) spinning PAN decomposes before melting.

Nylon-6 is made from

  1. adipic acid
  2. caprolactam
  3. hexamethylenediamine
  4. terephthalic acid
Show the answer

Answer: B. caprolactam Ring-opening polymerisation.

Drawing of fibres

  1. reduces strength
  2. orients chains, increasing strength
  3. adds colour
  4. removes catalyst
Show the answer

Answer: B. orients chains, increasing strength Draw ratio 3–5.

Theory questions

Describe the manufacture of polyester fibre with a flow diagram. (8 marks)

Show the model answer

PTA + MEG paste with Sb catalyst; esterification at 250–270 °C (water removed); pre-polycondensation 20–100 mbar; final polycondensation in disc-ring finisher < 1 mbar, 285 °C (MEG recovered); melt spinning through spinnerets with quench air; drawing, heat-setting, crimping/cutting (staple) or winding (POY/FDY).

Write a note on the manufacture of nylon-6,6. (4 marks)

Show the model answer

Adipic acid and hexamethylenediamine form nylon salt (1:1) in water; concentrated and polycondensed in autoclave/continuous reactor at 270–280 °C releasing water; melt extruded, cut to chips, melt spun and drawn. Uses: tyre cord, textiles, engineering plastics.

Frequently asked questions

How is synthetic fibres manufactured?

Polyester (PET) continuous polymerisation and melt spinning; nylon. Synthetic fibres are long-chain polymers spun into filaments. Polyester (polyethylene terephthalate, PET) is the largest; it is produced by esterifying purified terephthalic acid (PTA) with monoethylene glycol (MEG) and polycondensing the product under high vacuum at 280–290 °C with an antimony catalyst. The molten polymer is spun directly through spinnerets, cooled and drawn to orient the chains and develop strength. Nylon-6,6 is made by polycondensation of nylon salt (adipic acid + hexamethylenediamine), nylon-6 by ring-opening of caprolactam, and acrylic fibres by solution spinning of polyacrylonitrile.

What raw materials are used to make synthetic fibres?

PET: purified terephthalic acid (from p-xylene) and monoethylene glycol (from ethylene oxide); Catalysts and additives: Sb₂O₃/antimony acetate, TiO₂ (delustrant), stabilisers; Nylon-6,6: adipic acid + hexamethylenediamine; nylon-6: caprolactam; Acrylic: acrylonitrile (+ vinyl acetate), solvent DMF/NaSCN

What catalyst is used in synthetic fibres production?

antimony trioxide (polycondensation)

What is synthetic fibres used for?

Apparel and home textiles (blends with cotton/viscose); Industrial yarn, tyre cord, ropes, nets; PET bottles and films

Watch the animated P&ID →